Causes of Peeling During Shot Blasting of Aluminum Alloy Die Castings

Discover the main causes of peeling during the shot blasting of aluminum alloy die castings. Learn how process control and alloy quality affect casting performance with insights from Boyi Industry.

Overview of Aluminum Alloy Die Casting Process

The market for aluminum alloy die castings is growing larger, and with that, various issues arise during the die casting production process. So, what are the causes of peeling during shot blasting of aluminum alloy die castings?

Purpose of Shot Blasting in Aluminum Alloy Die Castings

Shot blasting of Aluminum Alloy Die Castings is done to further densify the castings, with a force of approximately 3 kilograms per square meter. If the aluminum alloy die castings have inherent quality issues during processing, peeling may occur during shot blasting. The following are some reasons:

Improper Mold or Injection Chamber Cleaning

1. The mold or injection chamber was not cleaned properly.

2. Insufficient injection pressure (also pay attention to whether there is any yielding of the moving mold during injection).

3. Problems with the gating system design, causing turbulence of the molten alloy as it enters the cavity.

4. Issues with mold temperature.

5. Severe splashing of molten metal during injection.

By analyzing these issues, solutions can be identified to control and prevent them, ensuring high-quality aluminum alloy die castings.