A zinc die casting can pass inspection before finishing and still bind during assembly. On a cosmetic component, the narrow slot behind a polished face may control the fit even though it attracts less attention than the visible surface. The drawing and approval plan must describe the finished mating geometry, including material removed during preparation and every coating layer added afterward.
Define the condition in which the drawing applies
State whether each critical dimension applies after casting, after mechanical preparation, or after the complete finish. For an assembly interface, specify the required finished condition and identify any intermediate dimensions needed to control production. A general finish note without a defined measurement condition leaves room for conflicting interpretations.
Identify the datum features used for inspection and whether they remain uncoated, become coated, or are machined later. If a datum surface changes during finishing, define how the final datum is established. A repeatable fixture must locate the part in the intended condition; a convenient pre-finish reference is not automatically the correct final reference.
Treat local material removal separately from coating buildup. Grinding, polishing and vibratory finishing can change surfaces and edge profiles, with restricted access inside small features. IZA identifies these access limits in its finishing guidance. Do not assume that preparation removes the same amount everywhere or that later coating restores the original geometry. [1] Coating is not a guaranteed remedy for substrate defects.

Use the total local coating stack
For a plated system, the dimensional allowance includes relevant strikes, underplates and final deposits, not only the named decorative top layer. Establish the total buildup at each mating face. Any additional topcoat affecting fit belongs in the dimensional review too.
Electroplating thickness varies with geometry and current distribution. Exposed regions and recesses can receive different deposits, and rack position can matter. A reading on an accessible cosmetic face does not establish thickness inside a slot. Agree the measurement locations and limits with the finisher rather than treating one average as a whole-part guarantee. [2]
Calculate the clearance before approving the finish
Consider a deliberately simplified planar slot and mating tab. After mechanical preparation, the slot width W is 10.10 ± 0.03 mm and the tab width B is 10.00 ± 0.02 mm. Assume each of the four opposing faces receives 15–25 μm of total deposit. These are hypothetical teaching values, not a recommended plating specification or a claimed manufacturing capability.
Let t1 and t2 represent deposits on the two slot faces, and t3 and t4 the deposits on the tab. The slot narrows while the tab grows. Final total width clearance is:
Cfinal = W − B − (t1 + t2 + t3 + t4)
| Condition | Calculation in mm | Clearance |
|---|---|---|
| Nominal | 10.10 − 10.00 − 4 × 0.020 | +0.020 mm |
| Minimum | 10.07 − 10.02 − 4 × 0.025 | −0.050 mm |
| Maximum | 10.13 − 9.98 − 4 × 0.015 | +0.090 mm |
All coating thicknesses are total deposit per face. 20 μm = 0.020 mm.
At the nominal dimensions and 20 μm per face, clearance is 0.020 mm. Combining the smallest slot, largest tab and maximum deposits gives −0.050 mm: interference. The opposite limits give 0.090 mm clearance.
This is a bound calculation, not a prediction of defect rate or yield. It assumes planar opposing faces and coating buildup only after the stated preparation stage. It excludes burrs, distortion, position error, further material removal and other effects. The result is total width clearance, not clearance on each side; do not transfer this formula directly to threads or other mating geometries.

Choose a control that preserves function and appearance
Masking functional faces can reduce buildup where clearance is limited. Define the coverage boundary, allowable coating encroachment and resulting protection requirements. A mask edge near a visible surface also needs an agreed appearance limit. Leaving a face uncoated changes its corrosion exposure and must be accepted for the application.
Precompensating the uncoated geometry can work when based on a validated local buildup range. Shifting the nominal dimension alone does not eliminate variation. Review the combined dimensional range before changing tooling or machining allowances, and agree demanding tolerances with the die caster. IZA specifically calls for close supplier involvement when unusually tight tolerances are required. [3]
Control the plating setup and check representative locations on the part and across the rack. Changes in orientation, loading or shielding should trigger review of the local thickness evidence. Do not recover a tight fit through uncontrolled polishing. Post-finish machining is an option only where approved: it can remove protective layers and alter the cosmetic boundary.
Verify the route on identifiable parts
Track identifiable trial parts after trimming, after mechanical preparation and after the full finish. Measure the same defined features and locations where practicable, recording the datum setup at each stage. These paired results help separate preparation loss from subsequent buildup instead of hiding both inside one final number.
Use suitable local coating measurements alongside dimensional inspection. ASTM B568 describes X-ray spectrometry as a noncontact method; its public scope explains that it measures coating mass per unit area, convertible to thickness when density is known. [4] Confirm the instrument, calibration, layer model and measurement access are suitable for the actual coating stack and feature. A thickness result is not proof of assembly fit.
Check the finished mating pair or an agreed functional gauge, with defined insertion depth and force where relevant. A go/no-go result verifies only the conditions represented by that gauge, not every geometric requirement. Approve cosmetic boundary samples and any required protection tests separately. Neither a smooth appearance nor an acceptable fit alone establishes coating performance.
For a drawing review, mark the critical finished dimensions, datum condition, mating surfaces, proposed finish stack and appearance boundaries. Use the Boyi contact page to discuss these requirements. Feasibility, measurement methods and acceptance limits must be established for the individual part.
General engineering guidance only. The example and diagrams do not establish a product specification, manufacturing capability or coating qualification.
Technical references
Sources support the principles marked in the text. The worked example and proposed review checks are original editorial guidance. Accessed 3 November 2026.
1 International Zinc Association Selecting the Right Finish
Mechanical preparation and access limits. No listed roughness values are adopted as product requirements.
2 Klein Plating Works Metal Electroplating 101
Layer sequence, current distribution and location dependent deposit thickness. Supplier guidance is not a universal specification.
3 International Zinc Association Design Rules
Supplier involvement for demanding tolerances. Historical numerical tolerance tables are not adopted.
4 ASTM International ASTM B568 98 reapproved 2021
Public scope and significance summary only. The full standard was not reviewed; the article does not claim compliance.